中国塑料 ›› 2015, Vol. 29 ›› Issue (02): 63-67.DOI: 10.19491/j.issn.1001-9278.2015.02.012

• 材料与性能 • 上一篇    下一篇

星形聚己内酯在聚乳酸中的增塑作用研究

申冰洁1,谢吉星1,张婷田盛益焦运红2   

  1. 1. 河北大学化学与环境科学学院2. 河北大学
  • 收稿日期:2014-06-06 修回日期:2015-01-21 出版日期:2015-02-26 发布日期:2015-02-26

Star Poly(ε-caprolactone) as a Nonmigrating flame retardant Plasticizer for Polylactide

  • Received:2014-06-06 Revised:2015-01-21 Online:2015-02-26 Published:2015-02-26

摘要: 以六羟基环三磷腈为引发剂,ε-己内酯(ε-CL)为原料,通过开环聚合反应合成了臂长为10的星状聚己内酯(SPCL),并将其作为阻燃增塑剂应用于聚乳酸(PLA)中,并与线型聚己内酯(LPCL)和乙酰柠檬酸三丁酯(ATBC)两种增塑剂进行了对比。实验结果表明,在添加20 份时SPCL,SPCL共混样品断裂伸长率达由纯PLA的7.40%增加到18.86%,优于相同分子量的LPCL但小于ATBC,同时SPCL共混样品的拉伸强度明显优于其他两种样品。热分析和氧指数数据表明,加入SPCL后可以提高PLA的阻燃性能,且对材料的结晶性能和热稳定性影响较小。与小分子ATBC相比,SPCL在聚乳酸的中迁出率接近为零,是一种良好的耐迁出增塑剂。

Abstract: Star-shaped poly(ε-caprolactone)(SPCL) was synthesized by ring-opening polymerization of ε-CL from hydroxyl end-capped cyclophosphazene initiators. The SPCL was used as flame-retardant plasticizers for polylactide(PLA) and compared with liner poly(ε-caprolactone)(LPCL) and acetyltributyl citrate(ATBC). The experiment data the plasticization efficiency of SPCL was higher than that of LPCL, but lower than that of ATBC. When 20 phr SPCL was added, the ultimate elongation of the PLA/SPCL composites increased from 7.40% to 18.86%. Meanwhile the tensile strength of the PLA/SPCL composites was obviously superior to the other composites. Thermo-gravimetric analysis (TGA) and limited oxygen index (LOI) results indicated that the addition of SPCL can promote the flame retardancy of the composites and had tiny effect on crystallinity and thermal stability of PLA. Migration tests showed that there no migration was determined for PLA/SPCL composites. Compared with ATBC SPCL, SPCL was an excellent nonmigrating plasticizer.