关键词: 流滴特效期, 检测方法, 聚乙烯流滴膜
Abstract: In this paper,a new test method for anti-fogging performance of greenhouse film of polyethy lene basedon the determination of surface tension was proposed. The relationship between the surface tension andtime of invalidation was formulated. A critical surface tension(34x10-3N/m) was set, below whichthe film was considered as invalidating During the test, the film was immersed in hot wa- terat 50℃ and the time lasted for the surface tension of the film decreased below the critical value was measured,which was considered measure of the time of invalidation.
张文龙, 戴亚杰, 刘阔, 陈宇. 聚乙烯流滴膜的流滴持效期快速判断方法研究[J]. 中国塑料, 2007, 21(2): 86-89.
ZHANG Wen-long, DAI Ya-jie, LIU Kuo, CHEN Yu. New Method for Fast Testing of Anti-fogging Time of Polyethylene Greenhouse Films[J]. China Plastics, 2007, 21(2): 86-89.
0 / / 推荐
导出引用管理器 EndNote|Ris|BibTeX
链接本文: https://www.plaschina.com.cn/CN/
https://www.plaschina.com.cn/CN/Y2007/V21/I2/86