Research on Thermal Decomposition Kinetics of Phenolic Resin Modified by Poly(ether ether ketone)

Limin WU Shuhua QI Nailiang LIU Shasha LI   

  • Received:2011-05-26 Revised:1900-01-01 Online:2011-09-26 Published:2011-09-26

Abstract: The behavior of thermal decomposition of poly(ether ether ketone) (PEEK) modified phenolic resin was investigated. The TG curves of PEEK modified PF could be divided into three stages. The thermal decomposition data was analyzed by Kissinger, Ozawa, and Crane equations. The obtained activation energy (E), pre-exponential factor (A), and reaction order (n) of the thermal degradation were 561 kJ/mol, 1.06×1035 s-1, 0.9648, repectively.

Key words: thermal decomposition, poly(ether ether ketone), phenolic resin, kinetics