Abstract: A new polyurethane membrane was prepared by a chain extending reaction of PVB and end-closed polyurethane prepolymer. The structure and performance of this membrane were investigated by FTIR, TG, DMA, and mechanical test. The new polyurethane membrane gave rise to good thermal stability. The content of TDI in the membrane was low and thus had a lower toxicity. Binding strength with polyamide fiber was increased to 58.58 N/2. 5 cm.